Polymer Property : Melting Point = 2036 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2036 °C
3697 °F
Zircar Refractory Composites RSMAT-3000 ALUMINA MAT
ZRCI Type RSMAT-3000 is a high purity, high temperature, flexible form composed of continuous 97% alumina ceramic fibers designed for use to 1650°C (3002°F). Type RSMAT-3000 contains little shot a..
Melting Point 2036 °C
3697 °F
Zircar Ceramics Alumina Mat
A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between..