Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 2040 °C | 3700 °F | |
MarkeTech Sapphire (Aluminum Oxide - Al2O3) Single Crystal Data provided by the supplier, MarkeTech International.Sapphire is grown by several methods: Boule form (Czochralski), in plate form, or as tubes, rods and plates. Boules are grown up to 8" diam.. |
|||
Melting Point | 2040 °C | 3700 °F | |
Mateck Sapphire Aluminium oxide Substrate, Al2O3 Substrate single crystals for superconductivity. |