Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 195 - 205 °C | 383 - 401 °F | Temperature range at which MFI = 10 g/10 min at 21.6 kg.; MQSA 111 |
Lubrizol Advanced Materials Pearlthane® ECO D20N55D Thermoplastic Polyurethane
(discontinued **) PEARLTHANE® ECO D20N55D is a 55 Shore D, High Performance natural TPU based on Renewable Sources with ca. 35% renewable content according to ASTM D6866 for Extrusion and Injection Molding applicati.. |
|||
Melting Point | 204 - 205 °C | 399 - 401 °F | |
Indium Corp. Indalloy® 254 86.9Sn/10.0In/3.1Ag Lead-Free Solder Alloy No Sn/In eutectic problem; potential use for flip chip assembly. Information provided by the manufacturer, Indium Corporation. |
|||
Melting Point | 183 - 205 °C | 361 - 401 °F | |
Indium Corp. Indalloy 114 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 195 - 205 °C | 383 - 401 °F | |
UBE 7024B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Melting Point | 195 - 205 °C | 383 - 401 °F | |
UBE 7034B Nylon 6/12 Copolymer Film Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal .. |
|||
Melting Point | 183 - 205 °C | 361 - 401 °F | |
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |