Thermal Properties Metric English Comments
Melting Point 2053 °C
3727 °F
Zircar Ceramics HC Sapphire (Single Crystal Aluminum Oxide) Hangar Clip
ZIRCAR hanger clips are comprised of sapphire (single crystal aluminum oxide) and are designed for use with hanger rod (HR-1). The single crystal structure of these clips prevents creep and deformat..