Melting Point 1213 - 1285 °C
2215 - 2345 °F
Kennametal Stellite Stellite® 3 PM cast
Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt..
Melting Point 1213 - 1285 °C
2215 - 2345 °F
Kennametal Stellite Stellite® 3 PM with P/M Processing
Typical applications include (aerospace) vane plugs, fuel metering pins, spacer bushings, (bearings) ball blanks, race blanks, (valve seat inserts) diesel engine exhaust, fluid valve seats, saw cutt..