Thermal Properties Metric English Comments
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.50 inch (12.7 mm) o.d. and 0.050 inch (1.27 mm) Thickness
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.50 in..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 0.75 inch (19.0 mm) o.d. and 0.065 inch (1.65 mm) Thickness
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 0.75 in..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Cold Drawn Tube, 3.50 inch (88.9 mm) o.d. and 0.219 inch (5.49 mm) Thickness
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Cold Drawn Tube, 3.50 in..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Cold Rolled Strip, 0.150 inch (3.81 mm) Thick
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.5 x 2.0 inch (13 x 51 mm)
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.5 x 2..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 0.62 inch (16 mm) Diameter
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 0.62 in..
Melting Point 1343 - 1377 °C
2449 - 2511 °F
Special Metals INCONEL® 690 Nickel Superalloy, Hot Rolled Flat, 2.0 inch (51 mm) Diameter
Composition adjustments for nuclear applications: 28-31 Cr; 0.04 max C; 0.10 max Co.Tensile strength (ultimate and yield) and elongation values reported here are typical for Hot Rolled Flat, 2.0 inc..