Melting Point 1380 - 1395 °C
2520 - 2543 °F
Kennametal Stellite Stellite® 250
Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace..
Melting Point 1380 - 1400 °C
2520 - 2550 °F
Special Metals BRIGHTRAY® Alloy C Electrical Resistance Alloy
A nickel-chromium electrical-resistance alloy for use at operating temperatures up to 2100°F (1150°C). It contains rare-earth additions for increased oxidation resistance, especially under co..
Melting Point 1380 °C
2520 °F
Goodfellow Iron 60/Titanium 40 Alloy
Information provided by Goodfellow.
Melting Point 1380 °C
2520 °F
Goodfellow Iron 91/Silicon 9 Alloy
Information provided by Goodfellow.