Melting Point 1450 - 1510 °C
2650 - 2750 °F
Crucible Steel 420 and 420F Chromium Steel
Crucible 416 Plus is a hardenable chromium steel which is the general purpose cutlery grade. This grade is magnetic in all conditions. Information provided by Crucible Specialty Metals.