Polymer Property : Melting Point = 27.5 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 27.5 °C
81.5 °F
3M FC-4400 Ionic Liquid Antistatic
3M™ Ionic Liquid Antistatic FC-4400 is a high purity antistatic additive compatible with a variety of high performance polymer systems.Features and Benefits:Optical ClarityNo metal or halogen ionsV..