Polymer Property : Melting Point = 270.0 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 132.2 °C
270.0 °F
DSC
Silon Tabond 3043 Adhesive Resin
TABOND 3043 is HDPE modified with maleic anhydride functional groups which promote bonding with different materials like polar polymers, metals and surface treated glass.Characteristics: • Stro..