Polymer Property : Melting Point = 2813 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1545 °C
2813 °F
American Elements Thulium Nanoparticles
General DescriptionThulium (Tm) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Thulium Particles are typically 25 - 100 nanometers (nm) with specifi..