Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 1710 °C | 3110 °F | |
American Elements Silicon Oxide Nanopowder General DescriptionSilicon Oxide (SiO2) Nanopowder, Silica Nanoparticles or nanodots are high surface area particles. Nanoscale Silicon Oxide Nanoparticles or Silica Particles are typically 5 - 100 .. |