Thermal Properties Metric English Comments
Melting Point 27.0 - 32.0 °C
80.6 - 89.6 °F
Dow TONE™ 0310 Polyol
TONE™ 0310 polyol is a very low melting tri-functional liquid polyol for use in polyurethane elastomers, coatings, adhesives and soft foams.Information provided by Dow