Melting Point
162
°C
323
°F
Primary; ASTM D3418
Fiberfil® PP-60/TC/15/VO/ND Polypropylene Homopolymer, 15% Talc Filled, Flame Retardant
Information provided by FIBERFIL Engineered Plastics