Polymer Property : Melting Point = 375 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 179 - 191 °C
355 - 375 °F
MQSA 111
Lubrizol Advanced Materials PEARLTHANE® 11T92EM Thermoplastic Polyurethane Elastomer
PEARLTHANE® 11T92EM is a polyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, combining hardness with excellent mechanical properties. It can be extrude..
Melting Point 182 - 191 °C
360 - 375 °F
Lucas-Milhaupt 60 Sn-40 Pb Tin/ Silver Solder
Applications and Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is d..