Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 180 - 192 °C | 356 - 378 °F | Huntsman/TMA |
Huntsman IROGRAN® A 89 E 4372 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melting Point | 183 - 192 °C | 361 - 378 °F | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 189 - 192 °C | 372 - 378 °F | |
Shandong Guangyin GYBHVN Polymer Our GYBHVN products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin |
|||
Melting Point | 189 - 192 °C | 372 - 378 °F | |
Shandong Guangyin GYBHVNP Polymer Our GYBHVNP products are mainly applied in fuel pipes and brake pipes of automobile and hoses of air conditioner.Information provided by Shandong Guangyin |