Polymer Property : Melting Point = 413 °F
Polymer Property :
Melting Point =
413 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Melting Point
210
-
212
°C
410
-
413
°F
Clariant 6008 L Nylon 6, High Impact, Injection Molding
Data provided by Clariant Masterbatches