Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 236 - 243 °C
457 - 469 °F
Nihon Superior 95A Sn-Sb Lead-Free Solder Alloy
Melting Point 236 °C
457 °F
Target; M2E-73-002
Indorama Ventures Mexico Polyclearâ„¢ T-94 PET Resin
Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de..