Polymer Property : Melting Point = 5160 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 2850 - 2900 °C
5160 - 5250 °F
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
Melting Point 2850 - 2900 °C
5160 - 5250 °F
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder
Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder ..
Melting Point 2850 - 2900 °C
5160 - 5250 °F
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder
A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u..
Melting Point 2850 - 2900 °C
5160 - 5250 °F
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder
Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced..
Melting Point 2850 - 2900 °C
5160 - 5250 °F
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder
Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi..