Thermal Properties Metric English Comments
Melting Point 49.0 - 54.0 °C
120 - 129 °F
Oceanchem Group Antioxidant 1076
Molecular Formula: C35H62O3Cas No.: 2082-79-3Property: This product is a nonpolluting nontoxic antioxidant with good heat-resisting and water-extracting performance.Characteristics and Uses: This pr..
Melting Point 49.0 - 54.0 °C
120 - 129 °F
Hong Kun Group AO 1076 Antioxidant
Chemical Name: 3-(3',5'-di-tert-Butyl-4'-hydroxyphenyl)propionic acid stearyl ester; Dibutylhydroxyphenylpropionic acid stearyl esterCAS No. 2082-79-3All information provided by Hongkun Group