Thermal Properties Metric English Comments
Melting Point 548 - 660 °C
1020 - 1220 °F
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Melting Point 548 - 660 °C
1020 - 1220 °F
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Melting Point >= 548 °C
>= 1020 °F
Solidus
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us..