Thermal Properties Metric English Comments
Melting Point 49.0 - 59.0 °C
120 - 138 °F
Fine Organics FINALUX G 728 Lubricant Additive
Applications: Internal and external lubricant for PVC cables, films, bottles, lead stabilized injection molded articles. Synergistic co-stabilizing properties with Pb-stabilizers.Information provid..