Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 316 °C | 600 °F | ASTM D1283 |
Solvay Specialty Polymers Ryton® P-6 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Melting Point | 316 °C | 600 °F | |
Heatbath/Park Scale Kleen 9 Descaling Salt A highly alkaline and oxidizing salt bath for metal descaling and the removal of ceramic shell material from ferrous and nickel alloy investment castings.Information provided by Heatbath Corporation.. |
|||
Melting Point | 316 °C | 600 °F | ASTM D1283 |
Solvay Specialty Polymers Ryton® V-1 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantApplications: CoatingsInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |
|||
Melting Point | 316 °C | 600 °F | ASTM D1283 |
Chevron Phillips Ryton® PR11 Polyphenylene Sulfide Coating Resin
(Unverified Data**) Characteristics: High temperatureNon-stickCorrosion resistantInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the Ryton product line. |