Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 316 °C | 601 °F | 10°C/min; ISO 11357-1/-3 |
EMS-Grivory Grivory® XE 4164 black 9225 PA*-GF30 Product description: Grivory XE 4164 black 9225 is a 30% glass fiber reinforced engineering thermoplastic material based on a semicrystalline, partially aromatic copolyamide. ISO polymer designation.. |