Thermal Properties Metric English Comments
Melting Point 310 - 316 °C
590 - 601 °F
DSC
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Melting Point 310 - 316 °C
590 - 601 °F
DSC
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..