Polymer Property : Melting Point = 620 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 605 - 620 °C
1120 - 1150 °F
Indium Corp. Indalloy 215 Silver Solder Alloy
Information Provided by Indium Corporation
Melting Point 605 - 620 °C
1120 - 1150 °F
Johnson Matthey Mattibraze 45 Cadmium Containing Silver Brazing Alloy
Safety Precautions with Cadmium Containing Alloys: Today the potential danger from cadmium fume is widely recognized. The localized extraction of fumes during brazing is now virtually obligatory. ..