Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 332 °C | 630 °F | ASTM D3418 |
Solvay Specialty Polymers Amodel® AF-4133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced
(discontinued AMODEL AF-4133 V0 is a 33% glass reinforced grade of polyphthalamide (PPA) resin that was designed specifically to process with water-cooled molds and meet the requirements of most electrical/electr.. |
|||
Melting Point | 332 °C | 630 °F | |
Asahi Glass Fluon® L169J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Melting Point | 332 °C | 630 °F | |
Asahi Glass Fluon® L170J PTFE Lubricant Fluon®PTFE lubricants are used as additive to plastics, rubbers, paints, greases and so on. Frictional resistance decreases and non-stick increases on the applied surface.Information provided by As.. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TFM™ 1600 PTFE Meets ASTM D4894 Type III, Grade 2 resinMolding and ram extrusion powder with very good free flowing propertiesGood metering propertiesGood mold filling behaviorImproved particle coalescenceDenser p.. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TFM™ 1700 PTFE Meets ASTM D4894 Type III, Grade 1 resinNon-free-flowing compression molding powderVery fine particle sizeDense polymer structure, low permeabilityImproved weldabilityLow deformation under loadGood .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TFM™ 1705 PTFE Non-free-flowing resinReduced, adjusted melt viscosityIncreased gel stabilityReduced cold flowLower porosity and permeabilityLower void contentExcellent non-stick and dielectric propertiesHigher ela.. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TF 1641 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TF 1750 PTFE Meets ASTM D4894 Type IINon-free-flowing powder gradeVery fine particle sizeGood electrical and mechanical propertiesLow molding pressureUsed in large billet moldingExcellent for production of very .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TFM™ 1630 PTFE
(discontinued **) Semi-free-flowing resin for convenient handlingHigh bulk density leading to more economical processingVery dense polymer structure; low permeabilityGood electrical and mechanical propertiesSmoother .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | Initial; ASTM D4894-98a |
3M Dyneon™ TFM™ X 1630 PTFE
(discontinued **) Semi-free-flowing resin for convenient handlingHigh bulk density leading to more economical processingVery dense polymer structure; low permeabilityGood electrical and mechanical propertiesSmoother .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TF 1645 PTFE Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed .. |
|||
Melting Point | 332 - 352 °C | 630 - 666 °F | initial; ASTM D4894-98a |
3M Dyneon™ TF 1620 PTFE Meets ASTM D4894 Type IV, Grade 2 resinSemi-free-flowing compression molding powderHigh bulk densityGood for large billets and thin walled isostatic moldingsVery dense polymer structure, similar to .. |
|||
Melting Point | 332 °C | 630 °F | ASTM D3417 |
Quantum PEEK Information provided by Quantum Advanced Engineering Plastics |