Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 380 °C | 716 °F | via DSC |
Specialty Coating Systems Parylene D Poly (P-Xylylene) Coating Parylene D is a polymer of para-xylylene modified by the substitution of chlorine atoms for two of the aromatic hydrogen atoms. Parylene D is similar in properties to Parylene C with the added abili.. |
|||
Melting Point | 380 °C | 716 °F | |
Parylene Coating Services D Poly (P-Xylylene) Monomer is dichloro para-xylylene. Parylene D is recommended where high temperature resistance is needed; it can be used up to 140°C where oxygen is present.Parylene is a generic name for poly-par.. |