Polymer Property : Melting Point = 73.3 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 73.3 °C
164 °F
Peak Melting Temperature; ExxonMobil Method
ExxonMobil Escorene® UL 7620 Adhesive Application Resin  (discontinued **)
Escorene Ultra UL 7620 is a medium flow rate, 24% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s..