Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 74.4 °C | 166 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil OPTEMA™ TC 140 Molding, extrusion, compounding and adhesive resin
(discontinued **) OPTEMA TC 140 is a high flow, 21.5% methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compou.. |