Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 826 °C | 1520 °F | |
American Elements Europium Nanoparticles General DescriptionEuropium (Eu) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Europium Particles are typically 10 - 45 nanometers (nm) with specif.. |