Polymer Property : Melting Point = 885.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 885.0 °C
1625 °F
IBC Advanced Alloys 10% BeCu Beryllium Copper Master Alloy
Beryllium copper “Master Alloys” are formulated to introduce relatively small percentage “alloying” additions to base metal furnace melts. Producers of aluminum, magnesium, and n..