Thermal Properties Metric English Comments
Melting Point 920 - 940 °C
1690 - 1720 °F
Wieland 1407 Wilaform Gold
Red gold for all kinds of decoration manufacturing.Applications: casting, chains, laminar decoration, pipes, tubingDental
Melting Point 920 - 950 °C
1690 - 1740 °F
Wieland 1601 Wilaform Gold
Soft yellow gold alloy, ideally for the production of strongly deformed parts in decoration manufacturing and for metal coinage.Applications: casting, chains, coin/shape, laminar decoration, pipes, ..
Melting Point 920 °C
1690 °F
American Elements Lanthanum Nanoparticles
General DescriptionLanthanum (La) Nanoparticles, nanodots or nanopowder are black spherical high surface area particles. Nanoscale Lanthanum Particles are typically 5 - 40 nanometers (nm) with speci..