Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 76.0 - 90.0 °C | 169 - 194 °F | |
Struktol TR 045 Processing Additive Oleochemical derivative with no metal ions.STRUKTOL® TR 045 is a fatty acid based additive designed to maximize the wetting to both a polar filler and a non-polar polymer. By wetting both surface.. |