Thermal Properties | Metric | English | Comments |
---|---|---|---|
Dropping Point | 204 °C | 400 °F | ASTM Test |
Lubriplate 1200-2 Lithium Type Multi-Purpose Grease This is a heavy-duty general purpose lithium type grease for both industrial and automotive applications. It provides a high film strength, shear stability, and AW & EP additives. Applications: Gene.. |
|||
Dropping Point | 204 °C | 400 °F | ASTM Test |
Lubriplate 1240 Lithium-Polymer Type Multi-Purpose Grease Highly water resistant and tacky, they are designed for applications were the grease is subjected to heavy pressure and shock loads. This series is available in 3 NLGI densities for a wide range of .. |
|||
Dropping Point | 204 °C | 400 °F | ASTM Test |
Lubriplate 1241 Lithium-Polymer Type Multi-Purpose Grease Highly water resistant and tacky, they are designed for applications were the grease is subjected to heavy pressure and shock loads. This series is available in 3 NLGI densities for a wide range of .. |
|||
Dropping Point | 204 °C | 400 °F | ASTM Test |
Lubriplate SFL-00 Aluminum Complex Synthetic Food Machinery Grade Grease This series provides an exceptionally wide operating temperature range, high shear stability, excellent water resistance, and load carrying properties. For use in freezers and other cold temperature.. |
|||
Dropping Point | 204 °C | 400 °F | |
ConocoPhillips Tacna® 2000 NLGI No. 2 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Dropping Point | 204 °C | 399 °F | ASTM D-566 |
ConocoPhillips ANDEROL® 783-00 Series Synthetic Food Grade Greases, NLGI Grade 00 Description: ANDEROL 783 Series Greases are made from synthetic hydrocarbons (PAO) and an aluminum complex soap thickener, allowing for a wide range of operating temperatures. The 783 Series Greases.. |
|||
Dropping Point | 204 °C | 400 °F | |
ConocoPhillips Tacna® 2000 NLGI No. 1 Description: Conoco Tacna 2000 is available in two NLGI grades: No. 1 and No. 2. The No. 2 grade is ideal for use in heavily loaded sleeve-type bushings and bearings subjected to shock loading and o.. |
|||
Dropping Point | 204 °C | 400 °F | ASTM Test |
Lubriplate Temp G.S. Low Lithium Based Grease For Open Gearing Lithium-based open gear grease made for all types of open gears. Available in 4 formulas for a variety of conditions and temperatures. Applications: Open gears, slides, fifth wheels, low temps. Gear.. |
|||
Dropping Point | >= 204 °C | >= 399 °F | ASTM D566, ISO 2176 |
Chesterton 710 Anti-Seize Compound Description: Chesterton® 710 Anti-Seize Compound is an anti-seize compound and assembly lubricant combining the high temperature, extreme pressure, and corrosion resistant properties of colloidal c.. |