Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 555 °C | 1030 °F | |
Ferro EG 2790 Metal Sealing Glass Type: Si-B Typical Powder Form: VSD Typical Application: Si Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for Kovar,.. |
|||
Annealing Point | 557 °C | 1030 °F | 10<sup>13</sup> dPa-s |
Schott D 263 Thin Borosilicate Glass D 263 is a low alkali borosilicate glass that is produced by melting the purest raw materials. As such, it is very resistant to chemical attack. D 263, with its specific properties and large rang.. |