Thermal Properties | Metric | English | Comments |
---|---|---|---|
Annealing Point | 1150 °C | 2100 °F | |
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Annealing Point | 1150 °C | 2100 °F | |
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |