Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Annealing Point = 1163 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 1163 °C
2125 °F
Momentive Performance Materials Type 254 Fused Quartz Tubing
A doped quartz material that blocks virtually all UV-B and UV-C radiation. Ideal for lamps requiring maximum visible transmittance with nearly complete UV protection. Including some quartz halogen ..