Thermal Properties Metric English Comments
Annealing Point 575 °C
1070 °F
Ferro EG 1001 Metal Sealing
Glass Type: Si-B Typical Powder Form: VSD Typical Application: Gun Mount Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched seals for..
Annealing Point 575 °C
1070 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8688 Borosilicate Glass
Borosilicate glass, highly UV-blocked, stabilized against solarization, sealing glass to Tungsten Backlights The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium..