Polymer Property : Annealing Point = 590 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 590 °C
1090 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8230 Intermediate sealing glass
The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG.