Annealing Point 445 °C
833 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
Annealing Point 445 °C
833 °F
Corning 9010 Alkali Barium Crushed Glass
Used for sealing and other applications.Information provided by Corning Incorporated.