Polymer Property : Annealing Point = 900 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 900 °C
1650 °F
Corning Vycor® 7904 Blue Glass
Absorbs yellow wavelengths and causes light transmitted through the glass to have a higher color temperature. Cobalt is introduced into the glass structure; therefore a lamp can be produced without..