Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Annealing Point = 995 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Annealing Point 995 °C
1820 °F
Corning Vycor® 7907 UV-Blocking Glass
Vycor-UV™ is cerium-doped and provides homogeneous absorption of UV-B and UV-C.Special Features:Superior optical qualityTight dimensional controlThermal and chemical properties ideally suited to hi..