Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, after 4000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, after 8000 hours exposure at 650°C (1200°F) Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed and 40% cold work Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 400 °C |
0.105 BTU/lb-°F @Temperature 752 °F |
|
Haynes 242® alloy, cold reduced sheet, annealed, 40% cold work, aged Age-hardenable, high ductility in the aged condition, lower thermal expansion than most alloys, very good oxidation resistance up to 815°C, excellent low cycle fatigue properties, very good therm.. |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Special Metals INCOLOY® Alloy 825 A nickel-iron-chromium alloy with additions of molybdenum and copper. It has excellent resistance to both reducing and oxidizing acids, to stress-corrosion cracking, and to localized attack such as.. |
|||
Specific Heat Capacity | 0.440 - 0.480 J/g-°C | 0.105 - 0.115 BTU/lb-°F | as built |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Specific Heat Capacity | 0.439 J/g-°C @Temperature 20.0 °C |
0.105 BTU/lb-°F @Temperature 68.0 °F |
|
Carlson 904L Austenitic Stainless Steel General Description904L is an austenitic nickel-chromium stainless steel with molybdenum and copper additions. The elevated nickel and chromium content of 904L make it resistant to corrosion in a w.. |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-28UH Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-35 Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-35H Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-38 Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-38SH Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-40SH Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-42M Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-42SH Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-44H Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-45 Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-45M Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-30EZ Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-33 Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-33SH Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-38H Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-38M Neodymium Iron Boron Magnetic Material |
|||
Specific Heat Capacity | 0.440 J/g-°C | 0.105 BTU/lb-°F | |
Alliance N-33M Neodymium Iron Boron Magnetic Material |