Thermal Properties Metric English Comments
Specific Heat Capacity 0.490 J/g-°C
0.117 BTU/lb-°F
Schott N-LASF41 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.490 J/g-°C
0.117 BTU/lb-°F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 538°C
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
Specific Heat Capacity 0.490 J/g-°C
0.117 BTU/lb-°F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
Specific Heat Capacity 0.490 J/g-°C
0.117 BTU/lb-°F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Annealed Strip/Sheet
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
Specific Heat Capacity 0.490 J/g-°C
0.117 BTU/lb-°F
TIMET TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Overaged
High-Strength, Oxidation Resistant Strip AlloyFeatures: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aer..
Specific Heat Capacity 0.490 J/g-°C

@Temperature 100 °C
0.117 BTU/lb-°F

@Temperature 212 °F
ATI Allegheny Ludlum AL 304DA Stainless/Carbon Steel Three-Ply Composite
Composition above represents only the Type 304 cladding. Its iron content calculated as balance.Allegheny Ludlum AL 304DA is tri-ply composite consisting of a dual stabilized, low carbon steel cent..