Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | Calculated |
Rogers Corporation RO3210 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Specific Heat Capacity | 0.790 - 0.830 J/g-°C | 0.189 - 0.198 BTU/lb-°F | |
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Specific Heat Capacity | 0.790 - 1.00 J/g-°C | 0.189 - 0.239 BTU/lb-°F | Average value: 0.910 J/g-°C Grade Count:12 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Schott LITHOSIL-Q Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Schott N-SF2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Schott P-SF8 Glass Suitable for precision moldingInformation Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Accuratus MACOR Machinable Glass Ceramic Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac.. |
|||
Specific Heat Capacity | 0.790 J/g-°C @Temperature 50.0 °C |
0.189 BTU/lb-°F @Temperature 122 °F |
|
Advanced Ceramics ZEMAT® ACL 2090 - Zero Expansion Glass-Ceramic “Zero Expansion” glass-ceramic is a transparent material now in production for applications requiring ultra-low thermal expansion. The primary crystal phase is a s-eucryptite (Li2OAl2O32SiO2) soli.. |
|||
Specific Heat Capacity | 0.790 J/g-°C | 0.189 BTU/lb-°F | |
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |