Polymer Property : Specific Heat Capacity = 0.206 BTU/lb-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Specific Heat Capacity 0.860 J/g-°C
0.206 BTU/lb-°F
Calculated
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S226 Aluminum Alloy, AlSi30CuMg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT)abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of p..
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6
Heat Treatment Condition T6 (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S232 Aluminum Alloy, AlSi17Fe4Cu3Mg, Condition T6x
Heat Treatment Condition T6x (Quench in water at RT). Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials all..
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T7
Heat Treatment Condition T7 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Specific Heat Capacity 0.860 - 0.900 J/g-°C
0.206 - 0.215 BTU/lb-°F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition T6
Heat Treatment Condition T6 (Quenching in water at RT)Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allo..
Specific Heat Capacity 0.860 J/g-°C
0.206 BTU/lb-°F
Schott N-KF9 Glass
Information Provided by SCHOTT North America, Inc.
Specific Heat Capacity 0.860 J/g-°C

@Temperature 1093 °C
0.206 BTU/lb-°F

@Temperature 1999 °F
ATI Allegheny Ludlum Altemp® HX Nickel-Based superalloy
Characteristics: outstanding resistance to oxidation at high temperatures, exceptional strength at elevated temperatures, good fabricability, good machinability in annealed condition, work hardening..