Thermal Properties Metric English Comments
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
calculated
Rogers Corporation RT/duroid® 6002 High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
calculated
Rogers Corporation RT/duroid® 6202 High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
calculated
Rogers Corporation RT/duroid® 6202PR High Frequency Laminate
Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric..
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
Calculated
Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Features and Benefits:Low dielectric lossExcellent mechanical properties versus temperature - reliable stripline and multi-layer board constructions.Uniform mechanical properties- ideal for multi-la..
Specific Heat Capacity 0.930 J/g-°C
0.222 BTU/lb-°F
DSC
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy