Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.35 J/g-°C | 0.323 BTU/lb-°F | DSC |
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico.. |