Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.423 J/g-°C | 0.3402 BTU/lb-°F | |
IBC Advanced Alloys Beralcast® 310 Beryllium-Aluminum Alloy This alloy, a metal matrix composite, consisting of between 60 and 70% Be (by weight) is a wrought product offered by IBC Engineered Materials to be used in the process of manufacturing extrusions f.. |